AMS 5719 ESR Refining Round bar, Flat bar
Specifications AMS 5719 datasheet, AMS 5719 Chemical, AMS 5719 Properties from Steelmelting (ESR refined), Blooming, Hot forging, Hot rolling, Heat treatment, Straightening, 100% Ultrasonic flaw detection test, Cold working or Machined. All of these mater
| Product parameters | |
| Material category:: | Martensitic Stainless Steel |
| Steel grade:: | AMS 5719C |
| Terms of price:: | Ex works, CIF, CFR |
| Stock & Inventory available:: | Diameter 50 ~ 230mm |
| Ultrasonic test standard:: | ASTM E2375 / MIL-STD- AMS 2154 / SEP 1923 / GB/T 4162 / EN 10228-3 / EN 10308 |
| Production lead time:: | Within 5 days after 30% deposit prepayable |
| Company ISO register No.:: | UQ211218R0 |
Description
AEROSPACE MATERIAL SPECIFICATION - Grade AMS 5719
TECHNICAL SPECIFICATIONS - AMS 5719C
OFFICIAL TEST CERTIFICATE - issued by TUV - SGS - BV
CHEMICAL COMPOSITION (mass weight - %)
C (%): 0.08 ~ 0.13
Si (%): ≤ 0.35
Mn (%): 0.50 ~ 0.90
P (%)≤: 0.020
S (%)≤: 0.015
Cr (%): 11.0 ~ 12.5
Mo (%): 1.50 ~ 2.00
Ni (%): 2.00 ~ 3.00
V (%): 0.25 ~ 0.40
N (%): 0.01 ~ 0.05
TYPICAL MECHANICAL PROPERTIES
Tensile strength, σb≥ /MPa: 1100
Yield strength, σs≥ /Mpa: 860
Elongation, δ5 ≥(%): 12.0
Hardness HBW: 341 ~ 375
Hardness HBS: 310 max in annealed condition
HEAT TREATMENT PRACTICE
Annealed: 691° C (+/-11) for 6 hours min followed by air cool
Hardened:1052° C (+/-) for 30 mins followed by oil quench
1st Tempered: 560-590° C for 1 hour min followed by air cool
2nd Tempered: 538-560° C for 3 hours min followed by air cool
MELTING PROCESS
The alloy is usually produced by BEF + AOD / EAF, followed by electroslag refining (ESR or VAR ) if necessary for special purpose.
TECHNICAL SPECIFICATIONS - AMS 5719C
OFFICIAL TEST CERTIFICATE - issued by TUV - SGS - BV
CHEMICAL COMPOSITION (mass weight - %)
C (%): 0.08 ~ 0.13
Si (%): ≤ 0.35
Mn (%): 0.50 ~ 0.90
P (%)≤: 0.020
S (%)≤: 0.015
Cr (%): 11.0 ~ 12.5
Mo (%): 1.50 ~ 2.00
Ni (%): 2.00 ~ 3.00
V (%): 0.25 ~ 0.40
N (%): 0.01 ~ 0.05
TYPICAL MECHANICAL PROPERTIES
Tensile strength, σb≥ /MPa: 1100
Yield strength, σs≥ /Mpa: 860
Elongation, δ5 ≥(%): 12.0
Hardness HBW: 341 ~ 375
Hardness HBS: 310 max in annealed condition
HEAT TREATMENT PRACTICE
Annealed: 691° C (+/-11) for 6 hours min followed by air cool
Hardened:1052° C (+/-) for 30 mins followed by oil quench
1st Tempered: 560-590° C for 1 hour min followed by air cool
2nd Tempered: 538-560° C for 3 hours min followed by air cool
MELTING PROCESS
The alloy is usually produced by BEF + AOD / EAF, followed by electroslag refining (ESR or VAR ) if necessary for special purpose.
Submit an enquiry for the displaying steel materials you are interested in TODAY!
Review